Atomic layer deposition of cobalt carbide films and their magnetic properties using propanol as a reducing agent

Authors

M. Sarr, N. Bahlawane, D. Arl, M. Dossot, E. McRae, and D. Lenoble

Reference

Applied Surface Science, vol. 379, pp. 523-529, 2016

Description

The investigation of highly conformal thin films using Atomic Layer Deposition (ALD) is driven by a variety of applications in modern technologies. In particular, the emergence of 3D memory device architectures requires conformal materials with tuneable magnetic properties. Here, nanocomposites of carbon, cobalt and cobalt carbide are deposited by ALD using cobalt acetylacetonate with propanol as a reducing agent. Films were grown by varying the ALD deposition parameters including deposition temperature and propanol exposure time. The morphology, the chemical composition and the crystalline structure of the cobalt carbide film were investigated. Vibrating Sample Magnetometer (VSM) measurements revealed magnetic hysteresis loops with a coercivity reaching 500 Oe and a maximal saturation magnetization of 0.9 T with a grain size less than 15 nm. Magnetic properties are shown to be tuneable by adjusting the deposition parameters that significantly affect the microstructure and the composition of the deposited films.

Link

doi:10.1016/j.apsusc.2016.04.096

Share this page: